Re: Tank Plating Bar???
Aluminium will conduct fine, however any splash that gets on the bar and drips back into the tank will drag aluminium into the solution. Chloride zinc will corode aluminium. Just make sure you keep the bar clean and dry. Not really a major issue.
Copper is usually used as it is one of the best conductors around.
Cheers
Mark
|