Quote:
Originally Posted by boxgods
Why glass it at all? Plastic water tanks get into the thousands of gallons size...
There is an very servicable plastic welder at harbor freight for $29 and a more usable one still for about $70. 1/4" polypropylene in 4' x 8' sheets can be had for about $75 if you shop a bit online.
|
Boxgods, to be honest as I was typing I more had a tank in mind that was not circular, I was in the mindset of a rectangular shape. Don't know why, just did

Obviously the walls of a flat tank are weaker than the wall of a circular one.
Depending on what shape most of your parts are would help to decide the shape of your tank. Of course long thin parts could be done in a round tank just a bit wasteful if thats all you do.
Just had another thought a steel frame could give the required strength to the walls of a flat sided tank as well.
Cheers M