Default Re: Anodize or Powder Coat?

I saw an episode of Orange County Choppers the other day where Pauly went to the PC company that is doing their stuff and applied the PC himself... I was surprised when they took an air blower and simply blew off unwanted areas of the powder before baking (at the serial number).
Also, the masks are applied first, then powder applied, then the mask pulled, then baked.
If you drill out the PC after baking, it will chip.