So did Paul Sr. kick his butt I kind of thought the PC would chip so thats why I asked. I thought the special tape they sell is for putting into the oven?? What other masks can be used besides the special tape. Regular painters tape, masking tape? And for the silicone plugs I guess you could use paper or wood as long as you pull them before baking? Is it best to use silicone plugs and leave them in on holes like spoke holes or pull the plugs as the powder won't run or move from where its sprayed?