got the Galv. from Reliance. They have a store close by & deliver for free. Inside is 18 ga. & the outside is 22 ga. they were something like $19 & $25 per sheet for 4' x 8'.
__________________
SouthWest Powderworx
Tyler Nutter
5054803934
www.swpowder.com