Thread
:
Looking for a Cheaper PC decoater??
View Single Post
#
4
(
permalink
)
05-20-2008, 12:56 AM
tr4dude
Newbie
Join Date: Nov 2007
Location: Sunny California
Posts: 29
Blog Entries:
3
Re: Looking for a Cheaper PC decoater??
a self cleaning oven will take it off if the parts can handle the heat.
__________________
Sonic Powder Coating
Sonic Coatings@aol.com
tr4dude