Hello
First i want to apologise for my english.I am from Romania(Europe)
I have buyed a wheel chroming kit from Casell INC.
I don't know what is the problem,i have the kit for 3 mounths.I didn't made not even a wheel until now!
I sundblast the wheel,polished,water break is OK.Degrease it,and zincate.After zincate i plate with Flash copper.I have agitation in the tank!I don't know what else can i do.Here is a picture with one wheel after flash copper

http://i305.photobucket.com/albums/n...n/SP_A0374.jpg

Please,i need some help.

Any sugestions??

Thanks

Ene Dan