Default Re: why brown before white polishing aluminum? PRO'S PLEASE READ

I'm with skidz on this one. I've had poor results with black on soft metals. The compound seems to scratch more than it polishes.

some stuff doesn't even like the brown it seems. I did this by going straight to white after wetsanding. They are cast aluminum wheels.

http://forum.caswellplating.com/phot...php?photo=2026