I've posted here before about my carter problem and after various preping methods, it came down to oil or water or dirt in the air lines. So I recently purchased a La-Man extractor/dryer that will remove down to 5 microns. Just tried 2 PC tests and both still have carters.
Is the 5 microns too big and should I have gone to a .01 micron filter??
Any help or suggestions would be appreciated.
Ben
|