Quote:
Originally Posted by benherr View Post
I've posted here before about my carter problem and after various preping methods, it came down to oil or water or dirt in the air lines. So I recently purchased a La-Man extractor/dryer that will remove down to 5 microns. Just tried 2 PC tests and both still have carters.

Is the 5 microns too big and should I have gone to a .01 micron filter??

Any help or suggestions would be appreciated.

Ben



Do you use any WD/40 in your shop??




I mean for any thing ......rusty bolts anywhere with in 50 feet of where you are powder coating...