Thread
:
Powder over Chrome???
View Single Post
#
10
(
permalink
)
05-22-2008, 09:02 PM
boston_jake01
Amateur Metal Finisher
Join Date: Oct 2006
Posts: 59
Re: Powder over Chrome???
I was wondering I have some chrome parts that are not in good shape I want to powder coat them with wet black I sand blasted and smooth the peeling areas how long do you think it would last on there
__________________
Rich
project 1
http://www.freewebs.com/boston_jake01/index.htm
boston_jake01
View Public Profile
Send a private message to boston_jake01
Visit boston_jake01's homepage!
Find all posts by boston_jake01