Thread: A big thanks
View Single Post
  #7 (permalink)  
Old 05-25-2008, 11:16 AM
welterracer welterracer is offline
Amateur Metal Finisher
 
Join Date: Sep 2007
Posts: 88
welterracer is on a distinguished road
Default Re: A big thanks

Ive only been doing this for about a year..

Its actually pretty easy.. hardest part is not being to extremely picky about how the parts turn out the first few times.. Dont get discouranged!

#1 you need a VERY good clean surface free from all Grease and oils..
(i like to blast all parts new or not to get maxiumum bonding)

I also like to preheat all my parts (unless its virgin steel) this helps get a little more powder on the parts and limits the waste of the powder.


Later

Brian
__________________
Halfbakedcoatings.com