Plating the rear plates on my 4 bl. carb., just started my new copy cad system, parts are coming out great when wet,nice glossy shine to them, when they are drying the copy cad parts are turning white with swirl marks on them, any idea why??
Temp set at 130 degree,s plating at 1.8 volts with .9 amps. wondering could temp be to high??
|