If im understanding the question, you're asking if powder will stick to powder aswell as powder will stick to metal. It is from my experience, powder that is not fully cured, and than sprayed will be just fine, but cured powder will need to be scuffed up to increase surface area. Once again this is just my experience, im sure someone will give you a more precise answer. Good luck
|