I found some quartz heaters at the local hardware store on spring clearance. Two tubes each, mounted vertically, 1500w units. I paid $29 each for them. I've done two oil pans (too big for my oven) and had pretty good luck with them. I don't know how well they would work on tubular parts, but for relatively flat panel sheet metal parts they are working great. Just another low $$ idea. Good luck!