Got it CarWiz, thanks much. That's pretty much what Caswell said also through Tech Support. I'll just have to remove the existing anodizing first with the anodizing stripper.

Do you have experience using the anodizing stripper? I purchased it once from Caswell and used it for my AR upper and lower receivers but the package did not come with directions on how long to leave in the solution so I think I overdid it... End result was that the receiver got "eaten" away and was noticeably smaller at the end to the point where they would not mate correctly and had a lot of slop after.