Default Re: Green olive drab ph will not rise?? why??

Well after trying no less than 12 times this product just does not work for me, period!! glassbead a part, de greese it, etch it, wash off with distilled water then plate it for 25 min. set it in green drab solution, turns brown instead of green, wish this product worked like there yellow cad solution, its a snap. Please work on the solution caswell before i go bunkers!!