Quote:
Originally Posted by viper56
Hi all,
Just flew back in last night and catching up on all of the posts. If you chose to use metal stud construction, make sure that you overlap the panels as shown on my website. It makes for a very sturdy design. Also for those of you who are looking for a low cost of cutting metal panels, Harbor Freight has electric metal shears for $29.00 which work great.
Jim
Oven Construction:
stivermotorsports.com
|
I clicked on your web address and when the site opens I click where it says powder coating oven plans and all I get is sponsor links. I am doing something wrong?
Harley