has anyone else had trouble with the heaters in the chromic acid. i put one heater in and it just fell apart( could have been a defect need to call caswell), the second heater i put in the rubber that is on the bottom of the heater (the one caswell sells with the kit), the acid started to eat it away. whats the deal