When I first started, I used a set of propane IR heaters that are made for heating up rooms and areas on construction sites. They look similar to this.

I picked them up at a local Wal-Mart for about $60 I have used them to do all kinds of things, from truck bumpers to step bars and roll bars and still use them on such large items.