Quote:
Originally Posted by Harleydad
|
I see here they also recommend a clear coat on their single stage chrome...I have used both the SS chrome and the Ultimate chrome from them. They Ultimate chrome is the best I have seen yet, even better then NIC's so I quess I will stick with the Ultimate Chrome ..