Default Re: Looking for a Cheaper PC decoater??

I spoke with Matt from PBP.... he said it wasn't the same as the D-Zolve and need heat and a way to get under the powder to work.
He explained it would come off in sheets like conventional strippers and won't work at all if it gets down to 60F.
I would like to find a less expensive stripper that's as effective as the D-Zolve... doesn't look like that will happen.
We also tried some perma gasket gasket remover on some parts...it softened it a little and that was it.
YMMV