Location: BC, Canada
Posts: 75
Re: Does anyone use IRON PHOSPHAT??
We use a an iron phosphate from Henkel, it's rinsed afterwards just with fresh water. We also use a product for items that are too large to fit into the tanks using a hot water pressure washer.