Default I wonder if trying a flash of zinc plating first would work with pit stop

Am tempted to try this on my various pot metal repairs.

Sand blast
pit stop all minor pits
zinc plate with a reasonable amount of current.
0.5% nitric brighten/activate and then flash copper and build.

Perhaps Caswell staff could clarify one thing with the pit stop. the various descritions on the web site state "imediately plate". Is there an issue with degreasing the pit stop?