I really mean connecting the RO unit to the distilled water tank (used for cleaning between processes) via a pipe (making sure the RO unit was positioned above the level of the tank). Then putting an overspill on the tank so the clean water could be flowing through the tank constantly without any jiggery-pokery. It would in effect be constantly diluting the contents of the distilled water tank (assuming you have the tap to the RO unit turned on).

At the moment I never know how contaminated the distilled water tank is with chemicals dragged over from the other tanks.