Re: mother's mag polish ruins my shine
I decided to re-buff. Starting with the white I went over the piece thoroughly, and then with the red rouge I finished it out. This time the Mother's polish looked great.
I think I had not buffed out all of the scratches from the sanding, although I couldn't see them, and they were catching and holding the polish. Who really knows? Polishing is like women. Just when you think you know something about it, it gets you again.
|