View Single Post
  #3 (permalink)  
Old 11-10-2003, 09:27 PM
c_gismo c_gismo is offline
Newbie
 
Join Date: Oct 2003
Posts: 9
c_gismo
Default

If the brown will cut very fast, then maybe I should use the white. I'll be replating the 24k gold onto the silver, so the fact that the gold goes does not really matter. It is only something like 3-5 microns thick and it is wearing thin in some places.

The key question is: will the red or the blue get out visable scratches that feel smooth, or not?
Reply With Quote