Re: Few Questions For The Pros
So i've got my tank, its a 28 gallon bin from Walmart. I built a wooden case for it, sealed the edges with wood glue then caulking. On one side of it, i gave it about 10 extra inches of space and cut a whole for the A/C unit, it's digital and is fully adjustable from 66-86*F so it should work fine. I'm just afraid all this stuff running at the same time (D/C power supply, A/C, Pump) is going to blow a lot of fuses in my circuit breaker, haha. Well anyways, all i need now is a RO unit, which i have picked out, & a good water pump for agitation. I've been looking at Magnetic Drive Little Giants & similar pumps, i just have no idea how much GPH it should have. My tank is 28 gallon, like i said before.. I'm just afraid too much will turn this thing into a water fountain. Any advice on these matters would be appreciated, thanks!
|