Default weird fading around the edges

I've been getting a strange fading around the edges on some of my parts. I can't be positive that this is what's causing it, but it appears that when I pull certain parts out of the dye early on to check what the color looks like the areas that temporarily dry off don't want to absorb dye again when I put them back in the dye. They're only out of the tank for a few seconds and I've always been doing this with no problems so I can't figure out what the common denominator is.

Any help is appreciated,