I'm pretty much done with the inside of my tank, all i need to do is finish the supporting pvc bars i drilled the 2 holes for on each side. I'm going to build a 1/2 inch plywood case, fill it with insulation to help support the tank & to retain the temperature. Going to have an A/C stuck into one side with about a foot of leeway, should work great and is much cheaper than a chiller (for now).
Here is some eye candy:
Got my cathode all setup along with the water agitation.
http://img359.imageshack.us/img359/2...mess001ib8.jpg
Top view.
http://img150.imageshack.us/img150/4...mess002dq8.jpg
Dyes/Chemicals, using 2.5 Gal buckets my friend got me from Ralphs Italian Ice.
http://img209.imageshack.us/img209/4...mess003gy6.jpg
My work table.
http://img294.imageshack.us/img294/7...mess005yy3.jpg
The mess that i call my basement, thats all my area for anything paintball/anodizing related.
http://img209.imageshack.us/img209/9...mess004vy7.jpg
Tell me what you guys think!