Electroless kroming-did something Wrong
Finally got around to getting all the tanks and heaters for electroless Kroming. did my first piece today and it didn't come out very good, it fact it was pretty bad.
Polished T-6061 aluminum to high shine.
placed in SP Degrease bath at for about 60 seconds at 125 degrees
let drip dry
placed in Zincate bath at 75 degrees for about 20 seconds and let drip dry.
placed in nickel/cobalt bath for 1 hour at 175 degrees, but I think I had the mixture wrong as I had to add additional distilled water and chemicals as the level dropped from evaporation.
Piece came out very dark gray. Tried buffing but the coating(gray) was pretty bad and it didn't come out shinning.
Will need to dump the mixture and start out again from scratch.
Any suggestions from someone that's done the electroless Krome would be greatly appreciated.
ben
|