Quote:
Originally Posted by KCV6
Ben, did you thouroghly rinse off the sp degreaser prior to zincating? Did the zincate fizz violently? What did the zincated finish look like? Too much zincate can cause problems.
Mark
|
Didn't rinse the SP, didn't see that in the instructions. The Zincate did fizz for about 10 seconds and then I removed it. Color was a medium gray looking. I didn't rinse that either, just let drip dry.
Ben