Default Re: Electroless kroming-did something Wrong

Quote:
Originally Posted by CarWiz View Post
I can see how you missed the rinse. It's NUMBER 1 following the degreasing step. If you missed that, you probably missed the water break test too. What's the volume of your solution and the size of the item?

Try it again and follow the direction precisely. Including you solution volume and maximum load. It's a proven process. Even a caveman can do it.

Added: Checking the book I have, your plating solution wasn't hot enough. What does your book say?
CarWiz,
I stand corrected! that's always been one, well I'm sure I have more, problems. I don't read all the directions. In my haste to try something new I always rush it. Oh well, I always try and assemble something and only read the directions when I can't figure it out. Thanks CarWiz for reminding me to follow the directions, LOL.

ben