Hey guys,
With winter fast approaching and the sub zero temps we get here in eastern Washinton im looking to move my line indoors. Will there be any concerns with transporting my set-up down into the climate controled semi-finished basement? Will the fumes be too much for indoor anodizing? I can ventillate if need be but would like to avoide that.
My next question is about the lead GP plates. Im also looking to step my main acid tank up to a 18 gal rubbermade with a dedicated airation set-up, ect. Is there a specific formula for use in calculating the size of the GP plates required per gallon or something? Do I need larger plates for a larger tank? Also, can I leave the Lead plates in the solution premenantly?
Again Thanks guys!