Your cathode should be roughly the size of your biggest run possible. So lets say you have a 20 amp PS, your biggest run would be about 3.3 sq feet. So a 3x1 sheet of lead would be fine, 4x1 preferably. I don't use caswells GP plates so i don't know how big or thick they are.