Caswell Inc. - Metal Stripping Kit

Use caution when stripping from Pot Metal parts - if the part is pitted down to the pot metal, the acids will attack the pits and begin to dissolve the parts.
__________________
--
Lance Caswell
Caswell Inc
http://www.caswellplating.com
Need Support? Visit our online support section at http://support.caswellplating.com
Have A Web Site?
Why not join our affiliate program and earn 15% of all sales. Join at http://www.caswellplating.com/affiliate.htm

Please support the moderators on our site by leaving reputation for their helpful posts. Read more here.
Reply With Quote