Re: Can I touch-up this valve cover or do I have to start over?
What powder is it? If it's not high temp, sand the part with some 220 or 320 grit and blow it off with clean/dry air. Wipe it down with denatured alcohol, tack cloth and clean/dry air again. Just be sure the denatured alcohol has dried completely and shoot another coat.
|