my first coat-another surface prep q?
I was going to first de-grease, then glass bead the surface. My question is what should I clean the part with after the glass bead? I'll be doing aluminum & steel parts. If I do not use an iron phosphate wash for steel or a zinc chromate for aluminum could I use something like denatured alcohol to wipe the parts down & dry with compressed air?