I used a DVOM (Digital Volt Ohm Meter) to measure the amperage. The reason I am thinking about going to the other system is because I was able to get results with it. With the current system I am not getting anything. In fact now for some reason I cannot get my parts to even dye. Which would lead me to believe that it is not anodizing before. I did discover with my old setup the acide I used was 36% which was diluted 1:1 so what I was anodizing with was nearly straight battery acid. I think this has a lot to do with my consitancy problems. I know the LCD system is a good one, I just cannot get it to work.