Silvaspray is a thin layer of silver, topcoated with lacquer. It's not really durable, and it's not suitable for high heat applications. It's one of several options to make non-metallic parts look like chrome.
Silvaspray isn't meant to be a final coat. It strictly makes non-metallic parts conductive, so they can be plated. We haven't tried powder coating over Silvaspray.
|