True- and I should add too that if anyone uses a vinyl plotter for graphics, I have found that trimming the application tape close to the graphic is a good idea, as well. The adhesive doesn't appear to leave any residue on a part, but it still interferes with dye absorbing into the anodic layer. Handling by the racking is the ideal way to go, and it is worth using a couple of points of contact to make a more stable rack on the part where that is possible.