Default Re: Powder coating Magnesium

Quote:
Originally Posted by goincrzy View Post
I got a Magnesium Intake for my car and a hobby type pc gun an old electric kitchen oven. I've powdercoated steel parts and Aluminum parts but not Magnesium..

Is there anything different I have to do for this type of metal for the pc to coat good?
If it's a cast part Make sure and outgas for a good long time. If this is not a familiar process keep asking.......