Default Re: Powder coating Magnesium

magnesium intake... alcohol blower... sounds serious! we want pics!!

i've never done magnesium, but yeah, to outgas i'd probably try preheating at 450 for an hour, let cool, and shoot. maybe use outgas forgivng powder additive, too.