Thread: SPRAY BOOTH
View Single Post
  #5 (permalink)  
Old 11-27-2003, 09:07 AM
non-stick non-stick is offline
Experienced Metal Finisher
 
Join Date: Sep 2003
Location: CT-NY-NJ area
Posts: 359
non-stick
Default

Tile board is another fine idea,bud. Easy to wipe down and clean. I like it. Just make sure you have some sort of metal in there that's grounded is all. I'd definately say you are on the right track to success! Keep up the good work..... Russ