Thread
:
Powder Coating chipping?
View Single Post
#
7
(
permalink
)
12-02-2003, 10:40 PM
tomg552001
Experienced Metal Finisher
Join Date: Dec 2002
Location: NJ
Posts: 290
If the temp of the lamp won't go higher than 300, cure much longer. Depending on what you're curing, i'd go for a good 35-45 minutes or so. Or maybe 25-35 once it starts flowing. Better safe than sorry, and its hard to over cure powder at that temp.
tomg552001
View Public Profile
Send a private message to tomg552001
Visit tomg552001's homepage!
Find all posts by tomg552001