View Single Post
  #6 (permalink)  
Old 01-05-2009, 11:17 PM
xgenmods xgenmods is offline
Newbie
 
Join Date: Dec 2008
Posts: 20
xgenmods is on a distinguished road
Send a message via AIM to xgenmods
Default Re: Help... wont take dye

Quote:
Originally Posted by coopduc View Post
You also don't say much about the parts themselves. Are they newly machined from 6061 or previously anodized parts that you are re-doing?


Parts are newly machined fro 6061 aluminum less than 3 day old. There were deburred in a vibrating tumbler with plastic media.