Question 100% Gloss Clear over 60% Gloss Powder...

Was wondering if any of you guys have done this...

Extreme or 100% Gloss Clear over a 60% Gloss powder??

The reason I ask is because i have been having really good luck (knock on wood) with the 60% Black w/ outgassing additive already in it. I have a ton of customers that want Gloss Black. What will the 60% Black look like with 100% clear on top of it?? Good?? Like regular 100% gloss black?