I tried a splash for the first time today. I like the results. These are a single color splash, tomorrow I'll try a 2 color. I used toluene (sp) to remove the rubber cement. Let the parts soak for about 5 minutes, then used a toothbrush. The cement came off very easily. Here's the results.