View Single Post
  #13 (permalink)  
Old 01-14-2009, 06:46 PM
ed_denu ed_denu is offline
Metal Finishing Guru
 
Join Date: Jul 2006
Posts: 618
ed_denu will become famous soon enoughed_denu will become famous soon enough
Default Re: 3 2000W in a 4x4x6?

Quote:
Originally Posted by FigureLLC View Post
our new 3.5x3.5x6 with 12kw hits 400 in 12min. That's also with 6" insulation, which I used to better handle ceramic coating temps.
Looks like the new oven is working well for you.