I agree, no sealer will protect the polished parts from the elements. A clear coat like VHT will help but using the clear coat does dull the aluminum slightly. If i were you, i would spend the money on zoops seal or something similiar. If you do use the VHT, once the clear starts getting scratches you will need to chemically or phyically strip it, than repolish alltogether. Atleast with zoops seal, you can probally go straight to buffing and not have to strip anything which can damage your finish.
|